TWP® - Application Instructions |
    |
Surface Preparation
- New Wood:
It is necessary to allow new wood to age for up to six months before staining. Pressure treated wood should be allowed 12 months natural weathering before staining.
- Untreated Old Wood:
Can be revived to look new. Remove mildew and growth with a mild bleach and water solution followed by a 1500-2500 p.s.i. output power washer.
- Previously Stained Wood:
May require a chemical stripping or brightening agent combined with power washing to remove all of the old coating. When working with a power washer use caution to avoid excess fraying of the wood surface. Allow 36 to 48 hours of dry time before TWP® application.
TWP® Stain Application
- Mix stain thoroughly before & occasionally during use
- Apply TWP® by brush, pump sprayer, roller, or applicator pad
- Saturate surface with TWP®
- If needed, apply second coat wet on wet
- Do not let TWP® puddle
- Excessive product that does not penetrate may cause failure
- Overnight dry time depending on temperature and humidity
- Do not thin TWP®
- Cleanup with Mineral Spirits
- Do not apply below 50°F
- Coverage Rate: 200-400 sq. ft. per gallon
|